NECESSITY OF RUSSIAN NANOINDENTATION STANDARD BASE DEVELOPMENT
Edward Aslanyan, Peter Krasowski
-
Abstract:Over the past years a large number of papers have been published on the application of the nanoindentation method. These works describe various aspects of the nanoindentation method and provide a detailed overview of the characteristics of different hardware and software tools implementing this method. However, measurements taken under the same conditions and on the seemingly same samples often provide a significant discrepancy in the results on different instruments functioning according to the same principle. This paper discusses the issues of metrological support for the nanoindentation method in Russia.
-
Keywords:nanoindentation method, Martens hardness, primary standard machine
-
Download:
-
DOI:_unreg_tc5-2010.015
Event details:
-
IMEKO TC:TC5
-
Event name:HARDMEKO 2010
-
Title:11th HARDMEKO Conference: HARDMEKO 2010 (together with 21st TC3 Conference on Measurement of Force, Mass and Torque and 2nd TC22 Meeting on Vibration Measurement)
-
Place:Pattaya, THAILAND
-
Time:21 November 2010 - 25 November 2010