An Area Function Measurement Method Based on Indenter Geometry for Small-Depth Nanoindentation
Dongmei Ren, Yu Wan, Zhenyu Zhu, Xiaoyan Duan
-
Abstract:The measurement methods of area function that are commonly used in nanoindentation are summarized and analyzed. An area function determination method based on the geometry of indenter tip for very small indentation depth is proposed. It combines the advantages of the area function measurement method based on measurement of standard sample and that based on indenter geometry. Experiments have been carried out to examine the effect of the area function. It is shown that this area function measurement method can improve the measurement accuracy of indentation hardness and reduced modulus when the indentation depth is very small.
-
Keywords:area function, nanoindentation, indentation hardness, reduced modulus, measurement
-
Download:
-
DOI:_unreg_tc5-2017.005
Event details:
-
IMEKO TC:TC5
-
Event name:TC5 Conference 2017 - Measurement facing new challenges!
-
Title:
13th Conference on the Measurement of Hardness (together with 23rd TC3 Conference on the Measurement of Force, Mass and Torque and 4th TC22 Conference on Vibration Measurement)
-
Place:Helsinki, FINLAND
-
Time:30 May 2017 - 1 June 2017